| APPLICATIONS:
- Pulse
power devices
- Power
transformers
- Current
transducers
- Devices
requiring a square-loop high saturation
material
- Magnetic
Switches
BENEFITS:
- High
saturation induction
- Extremely
low core loss
- High
BH squareness
- Can
be annealed for medium to high
permeability
|
| General
Properties & Characteristics |
| ELECTROMAGNETIC |
|
| Saturation
Induction (Tesla) |
1.61
|
| Maximum
DC Permeability (µ): |
Annealed
(High Freq.)
|
300,000 |
As
Cast
|
>40,000 |
| Saturation
Magnetostriction (ppm) |
30 |
Electrical
Resistivity (µ -cm) |
135 |
| Curie
Temperature (°C) |
370 |
| |
| PHYSICAL |
| Thickness
(mils) |
0.70 |
| Standard
Available Widths |
|
| Minimum
(inches) |
0.10 |
| Maximum
(inches) |
2.0 |
| Density
(g/cc) |
7.32 |
| Vicker's
Hardness (50g Load) |
880 |
| Tensile
Strength (MPa) |
1,000-1,700 |
| Elastic
Modulus (GPa) |
100-110 |
| Lamination
Factor (%) |
>75 |
| Thermal
Expansion (ppm/°C) |
5.9 |
| Crystallization
Temperature (°C) |
480 |
| Continuous
Service Temp. (°C) |
125 |
|